Pink Opal - Dry
Dipping glaze for stoneware
Watch this product and we will notify you once it is back in stock.
Pink Opal - Dry
Description
Dipping glaze for stoneware. Fires between 1210 °C and 1280 °C (cone 5 to 10). Can be sprayed and used for oxidation, reduction, etc. Since clays can vary and have different properties, we recommend testing the glaze on a small piece of the clay you want to use. Different results at different temperatures. The bag contains powder that should be mixed with water according to the instructions. The bag contains 4,5 kg of powder and yields approximately 4,5 liters of finished glaze.
Video
Information
Cone 6 oxidation (1230°C): Pink Opal produces a desert rose pink that ranges from semi-translucent to fully opaque, depending on application thickness. Thin applications yield a clear glaze with hints of pink precipitate; heavier applications will create an opaque purple-pink gloss finish that can also form a whitish cast in select areas.
Cone 10 reduction (1280°C): Pink fades out entirely, leaving a transparent gloss with white pooling.

TIP: Vertical pieces best allow the glaze to flow and create a semi-transparent, rose veil. Body textures and features will still be visible through the glaze. Thinner application will provide a glossy transparent finish. Thicker application will provide light pink floating. Surface decoration will be visible under the glaze, but if you apply the glaze thick, it could blur your image.
Safety
Can be irritating, harmful to health, and environmentally hazardous.
Documents
Manual for mixing the glaze